Material Notes:
Starglas FX05032 is Polyethylene Resin with a Proprietary Additive (foaming agent for polyolefins)Information provided by Eurostar.
Physical Properties Metric English Comments
Density 1.17 g/cc
0.0423 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.014 cm/cm

@Thickness 4.00 mm
0.014 in/in

@Thickness 0.157 in
E2P method
Mechanical Properties Metric English Comments
Tensile Strength at Break 18.0 MPa
2610 psi
5 mm/min; ISO 527
Elongation at Break 1.0 %
1.0 %
5 mm/min; ISO 527
Tensile Modulus 2.00 GPa
290 ksi
1 mm/min; ISO 527
Flexural Strength 27.0 MPa
3920 psi
2 mm/min; ISO 178
Flexural Yield Strength 32.0 MPa
4640 psi
2 mm/min; ISO 178
Flexural Modulus 2.10 GPa
305 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 2.00 kJ/m²
0.952 ft-lb/in²
80x10x4; ISO 180/1A
Izod Impact, Unnotched (ISO) 5.00 kJ/m²
2.38 ft-lb/in²
80x10x4; ISO 180/1U
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 62.0 °C
144 °F
Flatw 80x10x4, sp=64 mm; ISO 75/Af
Processing Properties Metric English Comments
Zone 1 195 - 205 °C
383 - 401 °F
Zone 2 210 - 220 °C
410 - 428 °F
Zone 3 220 - 230 °C
428 - 446 °F
Melt Temperature 230 °C
446 °F
Mold Temperature 40.0 - 55.0 °C
104 - 131 °F
Drying Temperature 80.0 °C

@Time 7200 sec
176 °F

@Time 2.00 hour