Eurostar Starflam RFB247EX PA66/6, Glass Bead/Fiber Filled, Flame Retardant, Injection Molded

Category Polymer , Thermoplastic , Nylon , Nylon 6/66
Manufacturer Eurostar Engineering Plastics
Trade Name Starflam
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Eurostar Starflam RFB247EX PA66/6, Glass Bead/Fiber Filled, Flame Retardant, Injection Molded.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
RFB247EX is a Halogen Free and Red Phosphorous Free Flame Retardant, Glass Bead/ Glass Fiber Reinforced Polyamide 66/ Polyamide 6 Injection Molding ResinInformation provided by Eurostar.
Physical Properties Metric English Comments
Density 1.44 g/cc
0.0520 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.0040 - 0.0060 cm/cm

@Thickness 4.00 mm
0.0040 - 0.0060 in/in

@Thickness 0.157 in
E2P method
Mechanical Properties Metric English Comments
Tensile Strength, Yield 114 MPa
16500 psi
ISO 527
Elongation at Break 2.6 %
2.6 %
ISO 527
Flexural Strength 161 MPa
23400 psi
ISO 178
Flexural Modulus 7.60 GPa
1100 ksi
ISO 178
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 210 °C
410 °F
Edgew 120x10x4, sp=100 mm; ISO 75/Ae
Flammability, UL94 V-0

@Thickness 1.60 mm
V-0

@Thickness 0.0630 in
Processing Properties Metric English Comments
Zone 1 260 - 280 °C
500 - 536 °F
Zone 2 270 - 285 °C
518 - 545 °F
Zone 3 265 - 280 °C
509 - 536 °F
Melt Temperature 265 - 280 °C
509 - 536 °F
Mold Temperature 70.0 - 90.0 °C
158 - 194 °F
Drying Temperature 75.0 - 85.0 °C

@Time 14400 - 21600 sec
167 - 185 °F

@Time 4.00 - 6.00 hour
Moisture Content 0.20 %
0.20 %