Eurostar Staramide RF005Z PA66, 25% Glass Fiber, Injection Molded

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 30% Glass Fiber Filled
Manufacturer Eurostar Engineering Plastics
Trade Name Staramide
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Eurostar Staramide RF005Z PA66, 25% Glass Fiber, Injection Molded.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Starflam RF005Z is a 25% Glass Reinforced Polyamide 66 Injection Molding Resin (also known as Staramide RF1005E-BK82205)Information provided by Eurostar.
Physical Properties Metric English Comments
Density 1.32 g/cc
0.0477 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.0010 - 0.0030 cm/cm
0.0010 - 0.0030 in/in
on Tensile Bar; E2P method
Mechanical Properties Metric English Comments
Tensile Strength at Break 150 MPa
21800 psi
5 mm/min; ISO 527
Elongation at Break 2.8 %
2.8 %
5 mm/min; ISO 527
Flexural Strength 200 MPa
29000 psi
2 mm/min; ISO 178
Flexural Modulus 6.60 GPa
957 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 7.00 kJ/m²
3.33 ft-lb/in²
80x10x4; ISO 179/1eA
Izod Impact, Unnotched (ISO) 40.0 kJ/m²
19.0 ft-lb/in²
80x10x4; ISO 180/1U