Eurostar Staramide R1000IX2 PA66, Impact Modified, Injection Molded

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Impact Grade
Manufacturer Eurostar Engineering Plastics
Trade Name Staramide
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Eurostar Staramide R1000IX2 PA66, Impact Modified, Injection Molded.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Staramide R1000IX2 is an Impact Modified Polyamide 66 Injection Molding Resin (also known as Star X 1010)Information provided by Eurostar.
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.010 - 0.015 cm/cm

@Thickness 4.00 mm
0.010 - 0.015 in/in

@Thickness 0.157 in
E2P method
Mechanical Properties Metric English Comments
Tensile Strength, Yield 65.0 MPa
9430 psi
50 mm/min; ISO 527
Elongation at Break >= 40 %
>= 40 %
50 mm/min; ISO 527
Tensile Modulus 2.20 GPa
319 ksi
1 mm/min; ISO 527
Flexural Yield Strength 70.0 MPa
10200 psi
2 mm/min; ISO 178
Flexural Modulus 2.00 GPa
290 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 13.0 kJ/m²
6.19 ft-lb/in²
80x10x4; ISO 180/1A
Izod Impact, Unnotched (ISO) NB
NB
80x10x4; ISO 180/1U
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 160 °C
320 °F
Flatw 80x10x4, sp=64 mm; ISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi) 65.0 °C
149 °F
Flatw 80x10x4, sp=64 mm; ISO 75/Af
Processing Properties Metric English Comments
Zone 1 260 - 270 °C
500 - 518 °F
Zone 2 270 - 280 °C
518 - 536 °F
Zone 3 270 - 280 °C
518 - 536 °F
Melt Temperature 270 - 280 °C
518 - 536 °F
Mold Temperature 60.0 - 100 °C
140 - 212 °F
Drying Temperature 80.0 °C

@Time 14400 sec
176 °F

@Time 4.00 hour
Moisture Content 0.20 %
0.20 %