Material Notes:
Star L POM D36 is Molybdenum Disulfide Lubricated, POM Copolymer Injection Molding ResinInformation provided by Eurostar.
Physical Properties Metric English Comments
Density 1.42 g/cc
0.0513 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.026 - 0.034 cm/cm

@Thickness 4.00 mm
0.026 - 0.034 in/in

@Thickness 0.157 in
E2P method
Mechanical Properties Metric English Comments
Tensile Strength, Yield 60.0 MPa
8700 psi
ISO 527
Elongation at Break 31 %
31 %
ISO 527
Flexural Strength 70.0 MPa
10200 psi
ISO 178
Flexural Modulus 2.20 GPa
319 ksi
ISO 178
Izod Impact, Notched (ISO) 12.0 kJ/m²
5.71 ft-lb/in²
80x10x4; ISO 180/1A
Izod Impact, Unnotched (ISO) 110 kJ/m²
52.3 ft-lb/in²
80x10x4; ISO 180/1U
Thermal Properties Metric English Comments
Melting Point 169 °C
336 °F
ISO 3146
Deflection Temperature at 0.46 MPa (66 psi) 145 °C
293 °F
Edgew 120x10x4, sp=100 mm; ISO 75/Be
Processing Properties Metric English Comments
Zone 1 180 - 190 °C
356 - 374 °F
Zone 2 180 - 190 °C
356 - 374 °F
Zone 3 180 - 200 °C
356 - 392 °F
Melt Temperature 180 - 200 °C
356 - 392 °F
Mold Temperature 60.0 - 100 °C
140 - 212 °F
Drying Temperature 80.0 °C

@Time 14400 sec
176 °F

@Time 4.00 hour
Moisture Content 0.10 %
0.10 %