Eurofoam VUL 401 Polyurethane Foam

Category Polymer , Thermoset , Polyurethane, TS , Thermoset Polyurethane Foam, Unreinforced
Manufacturer Eurofoam s.r.l.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Eurofoam VUL 401 Polyurethane Foam.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Used for the production of springs and shock-absorbing details in the automobile industry, seals for trunks and joints for ball bearings, pressure barsInformation provided by Eurofoam s.r.l.
Physical Properties Metric English Comments
Density 0.400 g/cc
0.0145 lb/in³
ISO 845-88
Mechanical Properties Metric English Comments
Tensile Strength 4.50 MPa
653 psi
ASTM D 412
Elongation at Break >= 405 %
>= 405 %
ASTM D 412
Compressive Yield Strength 0.0170 MPa

@Strain 25.0 %
2.47 psi

@Strain 25.0 %
ASTM 1056/85
0.0820 MPa

@Strain 50.0 %
11.9 psi

@Strain 50.0 %
ASTM 1056/85
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 80.0 °C
176 °F
ASTM D 3575
Minimum Service Temperature, Air -30.0 °C
-22.0 °F
ASTM D 3575
Descriptive Properties Value Comments
Cellular Structure Closed
Color Brown
Declaration of Heavy Metal Absence Conform
RoHS2002/95/EC