Material Notes:
Polychloroprene foam rubber. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurofoam s.r.l.
Physical Properties Metric English Comments
Density 0.260 - 0.300 g/cc
0.00939 - 0.0108 lb/in³
ISO 845-88
Water Absorption <= 5.0 %
<= 5.0 %
ASTM D 1056
Mechanical Properties Metric English Comments
Hardness, Shore OO 50 - 60
50 - 60
ASTM D 2240
Tensile Strength 0.800 MPa
116 psi
ASTM D 412
Elongation at Break >= 120 %
>= 120 %
ASTM D 412
Compressive Yield Strength 0.0750 MPa

@Strain 25.0 %
10.9 psi

@Strain 25.0 %
ASTM 1056/85
Tear Strength 1.00 kN/m
5.71 pli
ASTM D 624
Compression Set 15 %

@Strain 50.0 %
15 %

@Strain 50.0 %
ASTM D 395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 85.0 °C
185 °F
ASTM D 3575
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
ASTM D 3575
Shrinkage <= 5.0 %

@Temperature 70.0 °C,
Time 605000 sec
<= 5.0 %

@Temperature 158 °F,
Time 168 hour
Linear; ASTM D 1204
Descriptive Properties Value Comments
Cellular Structure Closed
Color Black
Declaration of Heavy Metal Absence Conform
RoHS2002/95/EC
Fire Resistance MV22 302
Pass
Vulcanization Sulfur