Esstech X-958-7424 Tetrahydrofurfuryl Methacrylate, C9H14O3

Category Polymer , Thermoset , Methacrylate
Manufacturer Esstech
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Esstech X-958-7424 Tetrahydrofurfuryl Methacrylate, C9H14O3.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
THFMA is a polar methacrylate containing a five-membered heterocyclic group that works well as an adhesion promoter in anaerobic adhesive and other applications. Listed on the Toxic Substance Control Act List. CAS # 2455-24-5.Information provided by ESSTECH, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.035 g/cc
1.035 g/cc
Molecular Weight 170.208 g/mol
170.208 g/mol
Optical Properties Metric English Comments
Refractive Index 1.456
1.456
Processing Properties Metric English Comments
Moisture Content <= 0.20 %
<= 0.20 %
Descriptive Properties Value Comments
Acidity (% Methacrylic Acid) < 0.1
Color (APHA) < 100
HQ Inhibitor (ppm) 50-70
Purity (%) > 95