Esstech X-756-0000 1,3-Glycerol Dimethacrylate/Maleate Adduct, C15H18O8

Category Polymer , Adhesive
Manufacturer Esstech
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Esstech X-756-0000 1,3-Glycerol Dimethacrylate/Maleate Adduct, C15H18O8.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
GDMA maleate combines the reactivity of maleic acid and GDMA to create a novel adhesive. Not listed on the Toxic Substance Control Act List. CAS # 136876-03-04.Information provided by ESSTECH, Inc.
Physical Properties Metric English Comments
Molecular Weight 326.301 g/mol
326.301 g/mol
Descriptive Properties Value Comments
MeHQ Inhibitor (ppm) 50-250
Purity (%) 55-95