HEMA succinate is one alternative to existing dental adhesive systems. It combines the reactivity of succinic acid with the adhesive characteristics of HEMA. Not listed on the Toxic Substance Control Act List. CAS # 20882-04-6.Information provided by ESSTECH, Inc.
Physical Properties Metric English Comments
Molecular Weight 230.216 g/mol
230.216 g/mol
Descriptive Properties Value Comments
MeHQ Inhibitor (ppm) 50-250
Purity (%) 55-95