Esstech X-739-0000 Ethoxylated Bis Phenol A Dimethacrylate, C39H56O12

Category Polymer , Thermoset , Epoxy , Epoxy Cure Resin
Manufacturer Esstech
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Esstech X-739-0000 Ethoxylated Bis Phenol A Dimethacrylate, C39H56O12.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This form of EBPADMA has 8 units of ethoxylation. Increasing the ethoxylated chain length increases the mobility of the molecule and therefore it reactivity and degree of conversion. Listed on the Toxic Substance Control Act List. CAS # 41637-38-1.Information provided by ESSTECH, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.122 g/cc
1.122 g/cc
Viscosity 525 cP

@Temperature 25.0 °C
525 cP

@Temperature 77.0 °F
Molecular Weight 716.8 g/mol
716.8 g/mol
Optical Properties Metric English Comments
Refractive Index 1.518
1.518
Processing Properties Metric English Comments
Moisture Content <= 0.20 %
<= 0.20 %
Descriptive Properties Value Comments
Acidity (% Methacrylic Acid) < 0.05
MeHQ Inhibitor (ppm) 150-250
Purity (%) > 87