Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Equate EMDA-6200 HDPE Blow Molding Resin

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Blow Molding Grade
Manufacturer Equate
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Equate EMDA-6200 HDPE Blow Molding Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
EMDA-6200 grade is a high-density polyethylene copolymer resin designed for blow molding small to medium size bottles. It can be used on intermittent as well as continuous blow molding machines for high-speed production of high quality bottles. The bottles have excellent environmental stress cracking resistance and a good balance of rigidity and impact strength. They are easily trimmed and exhibit excellent surface attributes.Applications: EMDA-6200 is intended for producing containers of up to 10 liter capacity for packaging household and industrial chemicals (detergents, bleach, fabric softeners, etc.) toiletries, cosmetics and food products. It is also suitable for producing thin-walled parts and household items. In addition EMDA-6200 can also be used successfully for extruding sheets and profiles including corrugated drainage pipesInformation provided by Equate
Physical Properties Metric English Comments
Density 0.954 g/cc
0.0345 lb/in³
ASTM D792
Environmental Stress Crack Resistance 50 hour
50 hour
F50; ASTM D1693 B
Melt Flow 0.40 g/10 min

@Load 2.16 kg
0.40 g/10 min

@Load 4.76 lb
ASTM D1238
High Load Melt Index 29 g/10 min

@Load 21.6 kg
29 g/10 min

@Load 47.6 lb
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 27.0 MPa
3920 psi
ASTM D638
Elongation at Break 1140 %
1140 %
ASTM D638
Flexural Modulus 1.25 GPa
181 ksi
ASTM D790
Crush Resistance 50.0 kg
110 lb (mass)
41g Boston Round Quart Bottle; ASTM D2659
Thermal Properties Metric English Comments
CTE, linear 120 µm/m-°C
66.7 µin/in-°F
ASTM D969
Melting Point 135 °C
275 °F
Equate Test Method
Crystallization Temperature 112 °C
234 °F
Equate Test Method
Deflection Temperature at 0.46 MPa (66 psi) 70.0 °C
158 °F
ASTM D648
Vicat Softening Point 125 °C
257 °F
ASTM D1525
Brittleness Temperature <= -100 °C
<= -148 °F
ASTM D746
Processing Properties Metric English Comments
Zone 1 175 - 180 °C
347 - 356 °F
Zone 2 185 - 190 °C
365 - 374 °F
Zone 3 185 - 190 °C
365 - 374 °F
Zone 4 185 - 190 °C
365 - 374 °F
Adapter Temperature 185 - 190 °C
365 - 374 °F
Die Temperature 185 - 190 °C
365 - 374 °F
Melt Temperature 200 - 215 °C
392 - 419 °F
Intermittent Machines
215 °C
419 °F
90 RPM
220 °C
428 °F
130 RPM
Head Temperature 185 - 190 °C
365 - 374 °F
Copyright © lookpolymers.com All Rights Reserved