Material Notes:
EO-98HT is a one component, electrically and thermally conductive, snap cure, die attach epoxy. It was designed for IC plastic packaging of semiconductors, hybrid micro-electronics, and photonic device assembly.Information provided by Epoxyset Inc.
Physical Properties Metric English Comments
Density 3.50 g/cc
0.126 lb/in³
Viscosity 35000 - 55000 cP
35000 - 55000 cP
Mechanical Properties Metric English Comments
Hardness, Shore D 84
84
ASTM D2240
Shear Strength 23.0 MPa
3340 psi
Adhesive Bond Strength >= 8.27 MPa
>= 1200 psi
Lap Shear Strength
Thermal Properties Metric English Comments
CTE, linear 42.0 µm/m-°C
23.3 µin/in-°F
Thermal Conductivity 1.80 W/m-K
12.5 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air >= 200 °C
>= 392 °F
Minimum Service Temperature, Air -55.0 °C
-67.0 °F
Glass Transition Temp, Tg >= 110 °C
>= 230 °F
Electrical Properties Metric English Comments
Electrical Resistivity <= 0.000400 ohm-cm
<= 0.000400 ohm-cm
Processing Properties Metric English Comments
Cure Time 10.0 min

@Temperature 175 °C
0.167 hour

@Temperature 347 °F
120 min

@Temperature 125 °C
2.00 hour

@Temperature 257 °F