Material Notes:
EPOXIOHM-97M is one part, pure silver filled, high electrical conductivity, epoxy adhesive. It is designed for microelectronics chip bonding application.Information provided by Epoxyset Inc.
Physical Properties Metric English Comments
Density 3.20 g/cc
0.116 lb/in³
Viscosity 10000 - 15000 cP
10000 - 15000 cP
Mechanical Properties Metric English Comments
Hardness, Shore D 88
88
ASTM D2240
Shear Strength 23.0 MPa
3340 psi
Adhesive Bond Strength 8.96 MPa
1300 psi
Lap Shear Strength
Thermal Properties Metric English Comments
CTE, linear 56.0 µm/m-°C
31.1 µin/in-°F
Thermal Conductivity 2.00 W/m-K
13.9 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 200 °C
392 °F
Minimum Service Temperature, Air -55.0 °C
-67.0 °F
Glass Transition Temp, Tg 89.0 °C
192 °F
Electrical Properties Metric English Comments
Electrical Resistivity <= 0.000400 ohm-cm
<= 0.000400 ohm-cm
Processing Properties Metric English Comments
Cure Time 10.0 min

@Temperature 175 °C
0.167 hour

@Temperature 347 °F
120 min

@Temperature 125 °C
2.00 hour

@Temperature 257 °F