Material Notes:
EO-38M-3 is a two components, 100% solids silver-filled epoxy system designed specifically for chip bonding in microelectronic and optoelectronic applications. It is used for thermal management applications due to its high thermal conductivity.Information provided by Epoxyset Inc.
Physical Properties Metric English Comments
Density 3.20 g/cc
0.116 lb/in³
Viscosity 30000 - 35000 cP
30000 - 35000 cP
Mechanical Properties Metric English Comments
Hardness, Shore D 88
88
ASTM D2240
Shear Strength 24.0 MPa
3480 psi
Adhesive Bond Strength 11.7 MPa
1700 psi
Lap Shear Strength
Thermal Properties Metric English Comments
CTE, linear 56.0 µm/m-°C
31.1 µin/in-°F
Thermal Conductivity 2.00 W/m-K
13.9 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 200 °C
392 °F
Minimum Service Temperature, Air -55.0 °C
-67.0 °F
Glass Transition Temp, Tg 95.0 °C
203 °F
Electrical Properties Metric English Comments
Electrical Resistivity <= 0.000400 ohm-cm
<= 0.000400 ohm-cm
Processing Properties Metric English Comments
Cure Time 10.0 min

@Temperature 175 °C
0.167 hour

@Temperature 347 °F
120 min

@Temperature 125 °C
2.00 hour

@Temperature 257 °F
Pot Life >= 480 min
>= 480 min