Material Notes:
EO-21 is a two part, silver filled high electrical conductivity epoxy adhesive. It is designed to cure at room temperature or rapidly at elevated temperature and exhibits very excellent adhesion and bond strength to a wide variety of substrates.Information provided by Epoxyset Inc.
Physical Properties Metric English Comments
Density 3.00 g/cc
0.108 lb/in³
Viscosity 30000 cP
30000 cP
Mechanical Properties Metric English Comments
Hardness, Shore D 84
84
ASTM D2240
Shear Strength 24.0 MPa
3480 psi
Adhesive Bond Strength 11.4 MPa
1650 psi
Lap Shear Strength
Thermal Properties Metric English Comments
CTE, linear 49.0 µm/m-°C
27.2 µin/in-°F
Thermal Conductivity >= 2.00 W/m-K
>= 13.9 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 150 °C
302 °F
Minimum Service Temperature, Air -55.0 °C
-67.0 °F
Glass Transition Temp, Tg 68.0 °C
154 °F
Electrical Properties Metric English Comments
Electrical Resistivity 0.000400 ohm-cm
0.000400 ohm-cm
Processing Properties Metric English Comments
Cure Time 120 min

@Temperature 65.0 °C
2.00 hour

@Temperature 149 °F
1440 min

@Temperature 25.0 °C
24.0 hour

@Temperature 77.0 °F
Pot Life 120 min
120 min