Epoxyset Epoxibond EB-309 Low Expansion Epoxy Adhesive

Category Polymer , Adhesive , Thermoset , Epoxy , Epoxy Adhesive
Manufacturer Epoxyset
Trade Name Epoxibond
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Epoxyset Epoxibond EB-309 Low Expansion Epoxy Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
EB-309 is a highly filled, extremely low expansion, epoxy adhesive. This low out-gassing adhesive exhibits excellent wettability without preheating metal bonding surfaces and has a good dimensional stability and excellent chemical resistance.Information provided by Epoxyset Inc.
Physical Properties Metric English Comments
Density 1.72 g/cc
0.0621 lb/in³
Water Absorption 0.10 %
0.10 %
Mechanical Properties Metric English Comments
Hardness, Shore D 92
92
ASTM D2240
Adhesive Bond Strength 13.8 MPa
2000 psi
Lap Shear Strength
Thermal Properties Metric English Comments
CTE, linear 18.0 µm/m-°C
10.0 µin/in-°F
Maximum Service Temperature, Air 120 °C
248 °F
Minimum Service Temperature, Air -55.0 °C
-67.0 °F
Glass Transition Temp, Tg 82.0 °C
180 °F
Processing Properties Metric English Comments
Cure Time 60.0 min

@Temperature 93.0 °C
1.00 hour

@Temperature 199 °F
1440 min

@Temperature 25.0 °C
24.0 hour

@Temperature 77.0 °F
Pot Life 100 min
100 min