Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Epoxyset Epoxibond EB-109M-4 Unfilled Epoxy Adhesive

Category Polymer , Adhesive , Thermoset , Epoxy , Epoxy Adhesive
Manufacturer Epoxyset
Trade Name Epoxibond
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Epoxyset Epoxibond EB-109M-4 Unfilled Epoxy Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A two-component, unfilled, flexible epoxy adhesive used for bonding and small potting applications in the medical, electronics, and aerospace industries. EB-109M-4 puts low stress on fragile parts and is flexible for crack resistance where some rigid epoxies may not work.Information provided by Epoxyset Inc.
Physical Properties Metric English Comments
Density 1.16 g/cc
0.0419 lb/in³
Viscosity 300 - 600 cP
300 - 600 cP
Mechanical Properties Metric English Comments
Hardness, Shore D 70
70
ASTM D2240
Adhesive Bond Strength 9.65 MPa
1400 psi
Lap Shear Strength
Thermal Properties Metric English Comments
CTE, linear 70.0 µm/m-°C
38.9 µin/in-°F
Maximum Service Temperature, Air 105 °C
221 °F
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Glass Transition Temp, Tg 45.0 °C
113 °F
Optical Properties Metric English Comments
Refractive Index 1.54
1.54
Processing Properties Metric English Comments
Cure Time 180 min

@Temperature 65.0 °C
3.00 hour

@Temperature 149 °F
1440 min

@Temperature 25.0 °C
24.0 hour

@Temperature 77.0 °F
Pot Life 60 min
60 min