Epoxyset Epoxibond EB-103F Unfilled Epoxy Adhesive

Category Polymer , Adhesive , Thermoset , Epoxy , Epoxy Adhesive
Manufacturer Epoxyset
Trade Name Epoxibond
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Epoxyset Epoxibond EB-103F Unfilled Epoxy Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A two-component, unfilled, fast setting epoxy adhesive used for bonding and small potting applications in the medical, electronics, and aerospace industries. EB-103F has excellent bond strength to various substrates including most metals, ceramics, glass, wood, and some plastics.Information provided by Epoxyset Inc.
Physical Properties Metric English Comments
Density 1.16 g/cc
0.0419 lb/in³
Viscosity 5000 - 8000 cP
5000 - 8000 cP
Mechanical Properties Metric English Comments
Hardness, Shore D 70
70
ASTM D2240
Adhesive Bond Strength 17.2 MPa
2500 psi
Lap Shear Strength
Thermal Properties Metric English Comments
CTE, linear >= 50.0 µm/m-°C
>= 27.8 µin/in-°F
Maximum Service Temperature, Air 105 °C
221 °F
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Glass Transition Temp, Tg 60.0 °C
140 °F
Optical Properties Metric English Comments
Refractive Index 1.53
1.53
Processing Properties Metric English Comments
Cure Time 720 min

@Temperature 25.0 °C
12.0 hour

@Temperature 77.0 °F
Pot Life 15 min
15 min