Category Polymer , Thermoset , Epoxy , Epoxy, Thermally Conductive
Manufacturer Epoxy Technology
Trade Name EPO-TEK®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Epoxy Technology EPO-TEK® 930-1 Thermally Conductive, Electrically Insulating Epoxy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Material Description: A two part, thermally conductive, electrically insulating epoxy. It can be used for heat sinking semiconductor devices, hybrid microelectronics, optics or medical devices. It is a lower viscosity and smaller particle size alternative to EPO-TEK® 930.Information Provided by Epoxy Technology
Physical Properties Metric English Comments
Specific Gravity 1.03 g/cc
1.03 g/cc
Part B
1.40 g/cc
1.40 g/cc
Part A
Particle Size <= 20 µm
<= 20 µm
Viscosity 60000 - 80000 cP

@Temperature 23.0 °C
60000 - 80000 cP

@Temperature 73.4 °F
5 rpm
Mechanical Properties Metric English Comments
Hardness, Shore D 82
82
Tensile Modulus 5.47 GPa
793 ksi
Storage
Shear Strength 11.28 MPa
1636 psi
Lap
>= 23.4 MPa
>= 3400 psi
Die
Thermal Properties Metric English Comments
CTE, linear 28.0 µm/m-°C
15.6 µin/in-°F
Below Tg
96.0 µm/m-°C
53.3 µin/in-°F
Above Tg
Thermal Conductivity 1.07 W/m-K
7.43 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 200 °C
392 °F
Continuous
300 °C
572 °F
Intermittent
Minimum Service Temperature, Air -55.0 °C
-67.0 °F
Continuous
-55.0 °C
-67.0 °F
Intermittent
Glass Transition Temp, Tg >= 70.0 °C
>= 158 °F
Dynamic Cure 20—200°C /ISO 25 Min; Ramp -10—200°C @ 20°C/Min
Decomposition Temperature 412 °C
774 °F
Degradation Temperature
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+13 ohm-cm
>= 1.00e+13 ohm-cm
Dielectric Constant 3.99

@Frequency 1000 Hz
3.99

@Frequency 1000 Hz
Dissipation Factor 0.0040

@Frequency 1000 Hz
0.0040

@Frequency 1000 Hz
Processing Properties Metric English Comments
Cure Time 10.0 min

@Temperature 150 °C
0.167 hour

@Temperature 302 °F
minimum
360 min

@Temperature 80.0 °C
6.00 hour

@Temperature 176 °F
minimum
Pot Life 1440 min
1440 min
Shelf Life 12.0 Month

@Temperature 25.0 °C
12.0 Month

@Temperature 77.0 °F
Descriptive Properties Value Comments
Color Amber
Part B
White
Part A
Consistency Smooth paste
Mix Ratio By Weight 100:4
Number of Components Two
Thixotropic Index 3.8
Weight Loss 0.09%
200°C
0.5%
250°C
1.31%