Material Notes:
EnSolv-Ionic is the perfect direct replacement for TCE, Perchloroethylene, 1,1,1-Trichloroethane, HCFC-141b, Freon and other hazardous or discontinued vapor degreasing, ultrasonic and manual cleaning solvents. EnSolv-Ionic was developed to not only remove rosin flux, no-clean flux, oil, grease and wax contaminants, but also to remove residual halide salts, ions and other polar contaminants that often result in component failures. EnSolv-Ionic is a patented azeotropic mixture that can be distilled and reused through numerous cycles before it needs to be replaced. EnSolv-Ionic is compatible with all metals and many plastics and other materials typically cleaned in vapor degreasers or by other methods.Information provided by Enviro Tech International.
Physical Properties Metric English Comments
Specific Gravity 1.28 g/cc
1.28 g/cc
75°F (water = 1)
Density 0.00500 g/cc
0.000181 lb/in³
Vapor Density
Water Absorption <= 0.020 %
<= 0.020 %
Vapor Pressure 0.173 bar

@Temperature 25.0 °C
130 torr

@Temperature 77.0 °F
Thermal Properties Metric English Comments
Specific Heat Capacity 1.05 J/g-°C
0.250 BTU/lb-°F
Boiling Point 69.0 °C
156 °F
Flammability Test 3.8 - 9.5
3.8 - 9.5
vol% limits based on n-Propyl Bromide
Electrical Properties Metric English Comments
Dielectric Breakdown 21000 V
21000 V
AC
Descriptive Properties Value Comments
Acid Acceptance, as NaOH >0.19% by wt.
Acidity , as HCl < 0.0010% by wt.
Appearance Clear; free of suspended matter
Base Materials Meets ASTM D6368 Yes
Evaporation Rate (Butyl Acetate = 1) 4.6
Flash Point TCC None
Kauri Butanol Number 130