Material Notes:
Available in North America Features: General PurposeRoHS Compliant Form: Pellets Information provided by Entec
Physical Properties Metric English Comments
Specific Gravity 1.04 g/cc
1.04 g/cc
ASTM D792
Melt Flow 7.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
7.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 44.8 MPa
6500 psi
ASTM D638
Flexural Strength 78.6 MPa
11400 psi
ASTM D790
Flexural Modulus 3.39 GPa
492 ksi
ASTM D790
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 87.8 °C
190 °F
Unannealed; ASTM D648
Vicat Softening Point 103 °C
217 °F
Rate A (50°C/h), Loading 1 (10 N); ASTM D1525
Compliance Properties Metric English Comments
FDA Yes
Yes
FDA 21 CFR 177.1640