Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Entec Hypro™ PPC-T30 Copolymer Polypropylene, 30% Talc Reinforced

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 30% Talc Filler
Manufacturer Entec Engineered Resins
Trade Name Hypro™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Entec Hypro™ PPC-T30 Copolymer Polypropylene, 30% Talc Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Entec
Physical Properties Metric English Comments
Density 1.15 g/cc
0.0415 lb/in³
ASTM D792
Melt Flow 10.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
10.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 26.7 MPa
3870 psi
ASTM D638
Elongation at Break 25.0 %
25.0 %
ASTM D638
Elongation at Yield 8.00 %
8.00 %
ASTM D638
Flexural Strength 44.0 MPa
6380 psi
ASTM D790
Flexural Modulus 2.137 GPa
309.9 ksi
tangent; ASTM D790
Izod Impact, Notched 0.590 J/cm

@Thickness 3.17 mm
1.11 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 115 °C
239 °F
ASTM D648
Copyright © lookpolymers.com All Rights Reserved