Entec Hypro™ PPC-GF15 Natural Impact Polypropylene, 15% Glass Reinforced

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 20% Glass Fiber Filler
Manufacturer Entec Engineered Resins
Trade Name Hypro™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Entec Hypro™ PPC-GF15 Natural Impact Polypropylene, 15% Glass Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Entec
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
ASTM D792
Melt Flow 10.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
10.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 54.0 MPa
7830 psi
ASTM D638
Elongation at Break 5.00 %
5.00 %
ASTM D638
Flexural Modulus 2.276 GPa
330.1 ksi
1% Secant; ASTM D790
Izod Impact, Notched 0.135 J/cm

@Thickness 3.17 mm
0.253 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 146 °C
295 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 121 °C
250 °F
ASTM D648