Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Entec Hypro™ PP-HP12NS Homopolymer, 12 Melt Flow, Nucleated, Anti-stat, Injection Molding

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer Entec Engineered Resins
Trade Name Hypro™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Entec Hypro™ PP-HP12NS Homopolymer, 12 Melt Flow, Nucleated, Anti-stat, Injection Molding.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Homopolymer, 12 Melt Flow, Nucleated, Anti-stat, Injection MoldingInformation provided by Entec
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Linear Mold Shrinkage 0.014 cm/cm
0.014 in/in
ASTM D955
Melt Flow 12 g/10 min

@Load 2.16 kg,
Temperature 230 °C
12 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 38.0 MPa
5510 psi
ASTM D638
Elongation at Yield 8.0 %
8.0 %
ASTM D638
Flexural Modulus, 1% Secant 1807 MPa
262100 psi
ASTM D790
Izod Impact, Notched 0.320 J/cm

@Thickness 3.17 mm
0.599 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 116 °C
241 °F