Entec Hypro™ PP-CP0.5/10 Impact Copolymer, Fractional Melt Flow

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer Entec Engineered Resins
Trade Name Hypro™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Entec Hypro™ PP-CP0.5/10 Impact Copolymer, Fractional Melt Flow.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This is a high impact copolymer intended for use in blow molding, pipe, tubing, sheet and other extrusion applications.Information provided by Entec
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Melt Flow 0.50 g/10 min

@Load 2.16 kg,
Temperature 230 °C
0.50 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 28.0 MPa
4060 psi
ASTM D638
Elongation at Yield >= 500 %
>= 500 %
ASTM D638
Flexural Modulus, 1% Secant 1345 MPa
195100 psi
ASTM D790
Izod Impact, Notched NB

@Thickness 3.17 mm
NB

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 88.0 °C
190 °F
ASTM D648