Material Notes:
Available in North America Features: Food Contact Acceptable and Low DensityAgency Ratings: FDA 21 CFR 176.170, Table 2, Cond. B; Cond. C; Cond. D; Cond. E; Cond. F; Cond. G; Cond. H; and FDA 21 CFR 177.1520RoHS Compliant Form: Pellets Information provided by Entec
Physical Properties Metric English Comments
Specific Gravity 0.924 g/cc
0.924 g/cc
ASTM D792
Melt Flow 50 g/10 min

@Load 2.16 kg,
Temperature 190 °C
50 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 8.96 MPa
1300 psi
ASTM D638
Tensile Strength, Yield 11.7 MPa
1700 psi
ASTM D638
Elongation at Break 100 %
100 %
ASTM D638
2% Secant Modulus 0.345 GPa
50.0 ksi
ASTM D790
Thermal Properties Metric English Comments
Vicat Softening Point 97.8 °C
208 °F
Rate A (50°C/h), Loading 1 (10 N); ASTM D1525