Entec Hypel® PELD20/.920 LDPE

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Molded
Manufacturer Entec Engineered Resins
Trade Name Hypel®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Entec Hypel® PELD20/.920 LDPE.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Entec.
Physical Properties Metric English Comments
Density 0.920 g/cc
0.0332 lb/in³
ASTM D792
Linear Mold Shrinkage 0.010 - 0.050 cm/cm
0.010 - 0.050 in/in
0.125 in; ASTM D955
Melt Flow 20 g/10 min

@Load 2.16 kg,
Temperature 190 °C
20 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 8.27 MPa
1200 psi
ASTM D638
Tensile Strength, Yield 11.0 MPa
1600 psi
ASTM D638
Elongation at Break 90 %
90 %
ASTM D638
Flexural Modulus 0.228 GPa
33.0 ksi
2% Secant; ASTM D790
Thermal Properties Metric English Comments
Vicat Softening Point 90.0 °C
194 °F
Rate A, Loading 1 (10 N); ASTM D1525