Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ensinger XP-132 Compression Molded PI Compound, 15% Graphite Filled

Category Polymer , Thermoplastic , Polyimide, Thermoplastic , Thermoplastic Polyimide, Graphite Filled
Manufacturer Ensinger
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ensinger XP-132 Compression Molded PI Compound, 15% Graphite Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The XP-130 is an amorphous high performance thermoplastic with high permanent temperature and creep resistance as well as excellent bearing and wear properties, excellent long term thermal stability and creep resistance.The XP 130 Series of Polyimide is a non-melting high temperature thermoplastic with high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excellent wear resistance along with good chemical resistance.Applications:Thermal & electrical insulatorsSwitch PartsVacuum SealsPlug PartsChip CarriersHot glass gripper fingersBalls for control valvesHousing PartsWelding EquipmentInformation provided by Ensinger Special Polymers, Inc.
Physical Properties Metric English Comments
Density 1.40 g/cc
0.0506 lb/in³
ASTM D792
Filler Content 15 %
15 %
Mechanical Properties Metric English Comments
Hardness, Rockwell M 119
119
ASTM D785
Tensile Strength 96.5 MPa
14000 psi
ASTM D638
Elongation at Break 3.0 %
3.0 %
ASTM D638
Flexural Strength 101 MPa
14700 psi
ASTM D790
Descriptive Properties Value Comments
Color Dark Brown