Ensinger Tecatron® XP-63 Compression Molded PPS Compound, 50% Fiberglass

Category Polymer , Thermoplastic , Polyphenylene Sulfide (PPS) , Polyphenylene Sulfide (PPS) with 50% Glass Fiber Filler
Manufacturer Ensinger
Trade Name Tecatron®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ensinger Tecatron® XP-63 Compression Molded PPS Compound, 50% Fiberglass.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Ensinger Special Polymers has over twenty different grades of TECATRON PPS available. Custom formulations can be blended to suit specific applications. Compression molding is amenable to short run production and yields products which are homogenous with low process stress.TECATRON PPS is a highly crystalline high-temperature thermoplastic with an excellent balance of cost, temperature resistance, strength, chemical resistance and flame retardance. TECATRON PPS is often used when long-term high-temperature performance and dimensional stability are a must, even in the presence of aggressive chemicals.Applications:Fuel InjectorsManifoldsPumpsPistonsGearsV-Packing GasketsBearingsInformation provided by Ensinger Special Polymers, Inc.
Physical Properties Metric English Comments
Density 1.80 g/cc
0.0650 lb/in³
ASTM D792
Filler Content 50 %
50 %
Mechanical Properties Metric English Comments
Hardness, Shore D 88
88
ASTM D2240
Tensile Strength 36.5 MPa
5300 psi
ASTM D638
Elongation at Break 0.80 %
0.80 %
ASTM D638
0.80 %
0.80 %
Flexural Strain; ASTM D790
Tensile Modulus 9.65 GPa
1400 ksi
ASTM D638
Flexural Strength 57.9 MPa
8400 psi
ASTM D790
Flexural Modulus 10.3 GPa
1500 ksi
ASTM D790
Descriptive Properties Value Comments
Color Black