Ensinger Tecapeek® XP98 XRO Polyetheretherketone (PEEK), compression molded, 30% carbon fiber filled, x-ray opaque

Category Polymer , Thermoplastic , Polyketone , Polyetheretherketone (PEEK) , Polyetheretherketone, PEEK, Carbon Fiber Filled
Manufacturer Ensinger
Trade Name Tecapeek®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ensinger Tecapeek® XP98 XRO Polyetheretherketone (PEEK), compression molded, 30% carbon fiber filled, x-ray opaque.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
TECAPEEK™ high performance polymer, made from Victrex PEEK polymer, has successfully replaced glass, stainless steel and titanium in a growing range of medical applications. The material's exceptional combination of properties allow engineers and designers the ability to create cost-effective, innovative parts that exhibit outstanding wear, heat, electrical and chemical resistance. The TECAPEEK™ family is made up of materials for medical applications.TECAPEEK™ MT, unfilled pigmented medical grade PEEKTECAPEEK™ XP98, compression molded 30% carbon fiber filled PEEK (isotropic properties)TECAPEEK™ MT CF30, extruded 30% carbon fiber filled PEEKTECAPEEK™ Classic™, ISO 10993 certification by resin and extrusion lot of 30 days contactTECAPEEK™ Classix™ XRO-20 radio opaque grade with 20% BaSO4 addedThe TECAPEEK™ family of high performance plastics are high effective in the creation and manufacture of high quality medical instruments. Five separate grades, each with qualities to meet a wide range of requirements for the engineer and product designer.Information Provided by Ensinger Industries, Inc.
Thermal Properties Metric English Comments
Melting Point 340 °C
644 °F
Maximum Service Temperature, Air 260 °C
500 °F
continuous