Ensinger Tecapeek® XP-181 Compression Molded PPEK Compound, EWS Filled and Carbon Fiber Reinforced

Category Polymer , Thermoplastic , Polyketone , Polyetheretherketone (PEEK) , Polyetheretherketone, PEEK, Carbon Fiber Filled
Manufacturer Ensinger
Trade Name Tecapeek®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ensinger Tecapeek® XP-181 Compression Molded PPEK Compound, EWS Filled and Carbon Fiber Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in lower amounts of scrap, uniform physical properties and fewer molded-in stresses.TECAPEEK is a high-perfomance engineering thermoplastic. This semi-crystalline material has a balance of high temperature mechanical properties, chemical and steam resistance, superior wear properties and processability which makes it unique.Applications Include:Bearings and BushingsDown-hole instrumentationWear RingsBall Valve SeatsElectrical ComponentsBack-up and V-RingsPiston Rings and Rider BandsInformation provided by Ensinger Special Polymers, Inc.
Physical Properties Metric English Comments
Density 1.90 g/cc
0.0686 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Rockwell M 104
104
ASTM D785
Tensile Strength 84.8 MPa
12300 psi
ASTM D638
Elongation at Break 1.1 %
1.1 %
ASTM D638
1.8 %
1.8 %
Flexural Strain; ASTM D790
Tensile Modulus 10.3 GPa
1500 ksi
ASTM D638
Flexural Strength 132 MPa
19200 psi
ASTM D790
Flexural Modulus 9.65 GPa
1400 ksi
ASTM D790
Izod Impact, Notched 0.374 J/cm
0.700 ft-lb/in
ASTM D256
Descriptive Properties Value Comments
Color Black