Ensinger Tecapeek® XP-111 Compression Molded PEEK Compound, 50% Carbon Fiber

Category Polymer , Thermoplastic , Polyketone , Polyetheretherketone (PEEK) , Polyetheretherketone, PEEK, Carbon Fiber Filled
Manufacturer Ensinger
Trade Name Tecapeek®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ensinger Tecapeek® XP-111 Compression Molded PEEK Compound, 50% Carbon Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in lower amounts of scrap, uniform physical properties and fewer molded-in stresses.TECAPEEK is a high-perfomance engineering thermoplastic. This semi-crystalline material has a balance of high temperature mechanical properties, chemical and steam resistance, superior wear properties and processability which makes it unique.Applications Include:Bearings and BushingsDown-hole instrumentationWear RingsBall Valve SeatsElectrical ComponentsBack-up and V-RingsPiston Rings and Rider BandsInformation provided by Ensinger Special Polymers, Inc.
Physical Properties Metric English Comments
Density 1.49 g/cc
0.0538 lb/in³
ASTM D792
Filler Content 50 %
50 %
Water Absorption 0.13 %

@Time 86400 sec
0.13 %

@Time 24.0 hour
ASTM D570
Crystallinity 17 %
17 %
Mechanical Properties Metric English Comments
Hardness, Rockwell M 110
110
ASTM D785
Tensile Strength 129 MPa
18700 psi
ASTM D638
Elongation at Break 1.1 %
1.1 %
ASTM D638
1.5 %
1.5 %
Flexural Strain; ASTM D790
Tensile Modulus 17.9 GPa
2600 ksi
ASTM D638
Flexural Strength 214 MPa
31000 psi
ASTM D790
Flexural Modulus 17.9 GPa
2600 ksi
ASTM D790
Compressive Strength 276 MPa
40000 psi
10% Deformation; ASTM D695
Compressive Modulus 4.90 GPa
710 ksi
ASTM D695
Izod Impact, Notched 0.742 J/cm
1.39 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 343 °C
649 °F
DSC
Descriptive Properties Value Comments
Color Black