Ensinger Tecaform™ AH ID Metal Detectable Acetal Copolymer (POM)

Category Polymer , Thermoplastic , Acetal (POM)
Manufacturer Ensinger
Trade Name Tecaform™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ensinger Tecaform™ AH ID Metal Detectable Acetal Copolymer (POM).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
TECAFORM™ AH ID is the fist commercially available acetal that is fully detectable by standard metal detection equipment. Exhibiting excellent machinability and a good combination of physical properties along with FDA compliance, TECAFORM AH ID is ideal for enhancing product safety in food processing applications.
Physical Properties Metric English Comments
Specific Gravity 1.48 g/cc
1.48 g/cc
ASTM D790
Water Absorption 0.22 %

@Time 86400 sec
0.22 %

@Time 24.0 hour
ASTM D570
Water Absorption at Saturation 0.65 %
0.65 %
ASTM D570
Mechanical Properties Metric English Comments
Hardness, Rockwell M 86
86
ASTM D785
Tensile Strength, Yield 64.0 MPa
9280 psi
ASTM D638
Elongation at Break 25 %
25 %
ASTM D638
Tensile Modulus 2.80 GPa
406 ksi
ASTM D638
Flexural Strength 75.8 MPa
11000 psi
ASTM D790
Flexural Modulus 2.48 GPa
360 ksi
ASTM D790
Compressive Strength 31.0 MPa
4500 psi
ASTM D695
Izod Impact, Unnotched 0.534 J/cm
1.00 ft-lb/in
ASTM D256
Coefficient of Friction, Dynamic 0.21
0.21
40 psi, 50 fpm; ASTM D3702
K (wear) Factor 131 x 10-8 mm³/N-M
65.0 x 10-10 in³-min/ft-lb-hr
40 psi, 50 fpm
Limiting Pressure Velocity 0.0507 MPa-m/sec
1450 psi-ft/min
ASTM D792
Thermal Properties Metric English Comments
CTE, linear 110 µm/m-°C
61.0 µin/in-°F
ASTM D696
Melting Point 165 °C
329 °F
ASTM D2133
Maximum Service Temperature, Air 100 °C
212 °F
Continuous; UL746B
141 °C
285 °F
Intermittent
Deflection Temperature at 0.46 MPa (66 psi) 158 °C
316 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 110 °C
230 °F
ASTM D648
Flammability, UL94 HB
HB
UL 94
Electrical Properties Metric English Comments
Surface Resistivity per Square 1.00e+12 ohm
1.00e+12 ohm
ASTM D257