Ensinger TECATOR™ GF30 (XP142T) Polyamide-imide (PAI), 30% glass filled, compression molded

Category Polymer , Thermoplastic , Polyamide-imide (PAI) , Polyamide-Imide, Glass Filled , Polyamide-Imide, Molded
Manufacturer Ensinger
Trade Name TECATOR™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ensinger TECATOR™ GF30 (XP142T) Polyamide-imide (PAI), 30% glass filled, compression molded.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
TECATOR™ is a high performance melt processable polyamideimide that maintains its excellent mechanical and wear properties in temperature environments exceeding 500°F. Stock shapes from Ensinger are available in three grades: TECATOR™ TI 5013, high strength structural grade featuring good electrical properties and strength, making it ideal for demanding applications at a broad range of temperatures. TECATOR™ TI 5031 offers high PV capabilities in bearing applications, primarily at high loads and low speeds. TECATOR™ GF30 (XP1424T) is a 30% glass filled grade, compression molded with superior stiffness and dimensional stability. It is available in a wide variety of custom tube, ring, rod and plate sizes.Excellent weather and gamma radiation resistanceOutstanding bearing wear properties (at elevated temperatures, TECATOR™ TI 5031 offers superior wear rates)High strength and stiffnessExcellent electrical valuesGood chemical resistance (TECATOR™ is not attacked by common solvents or fuels and is acceptable for use in contact with many acids)Maintains a high proportion of mechanical properties over a broad temperature spectrum - cryogenic to 500°FTECATOR™ TI 5013 and TI 5031 are available in a wide variety of metric sizes in rod and plateTECATOR™ (PAI) typical applications: Pump parts, valve seats, piston rings, seal rings, engine transmission parts and bearing cages. For the semiconductor industry it is used for "burn in" test sockets, nests, chassis and other applications such as welding nozzle tips.Information Provided by Ensinger Industries, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.58 g/cc
1.58 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Rockwell M 116
116
ASTM D785
Tensile Strength at Break 117 MPa

@Temperature 22.8 °C
17000 psi

@Temperature 73.0 °F
ASTM D638
Elongation at Break 2.0 %

@Temperature 22.8 °C
2.0 %

@Temperature 73.0 °F
ASTM D638
Flexural Strength 145 MPa

@Temperature 22.8 °C
21000 psi

@Temperature 73.0 °F
ASTM D790
Flexural Modulus 5.66 GPa

@Temperature 22.8 °C
821 ksi

@Temperature 73.0 °F
ASTM D790
Izod Impact, Notched 0.400 J/cm

@Temperature 22.8 °C
0.750 ft-lb/in

@Temperature 73.0 °F
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 38.0 µm/m-°C
21.1 µin/in-°F
ASTM D696
Maximum Service Temperature, Air 260 °C
500 °F
continuous
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Dielectric Constant 3.8

@Frequency 1.00e+6 Hz
3.8

@Frequency 1.00e+6 Hz
ASTM D150
4.3

@Frequency 2.00e+7 Hz
4.3

@Frequency 2.00e+7 Hz
ASTM D150
4.4

@Frequency 3.00e+7 Hz
4.4

@Frequency 3.00e+7 Hz
ASTM D150
Dielectric Strength 17.7 kV/mm
450 kV/in
ASTM D149
Dissipation Factor 0.0050

@Frequency 2.00e+7 Hz
0.0050

@Frequency 2.00e+7 Hz
0.0060

@Frequency 1.00e+6 Hz
0.0060

@Frequency 1.00e+6 Hz
0.0080

@Frequency 3.00e+7 Hz
0.0080

@Frequency 3.00e+7 Hz