Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ensinger TECASINT 8001 Polytetrafluoroethylene (PTFE) + Polyimide, 20% (PI)

Category Polymer , Thermoplastic , Fluoropolymer , PTFE , Polyimide, Thermoplastic
Manufacturer Ensinger
Trade Name TECASINT
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ensinger TECASINT 8001 Polytetrafluoroethylene (PTFE) + Polyimide, 20% (PI).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excellent wear resistance among other things. The TECASINT 2000 series offers these enhanced thermal properties along with lower moisture absorption, a higher degree of toughness, and better machining properties. TECASINT 2011 is unfilled, while TECASINT 2021 contains 15% graphite which offer improved wear resistance and a lower coefficient of friction. TECASINT 2000 series with their superior physical properties, are ideal for application in the aerospace, nuclear, automotive, electrical/electronics, and chemical processing industries.Main FeaturesAntiadhesiveStrongGood chemical resistanceVery good UV and weather resistanceFlame retardant according to UL94 V-0Very toughVery good electrical insulationGood slid and wear propertiesEasily machinedApplicationsMechanical engineeringFittingsCryogenicsMedical technologyConveyor technologyElectrical engineeringFood technologyTextile industryPreferred FieldsValve seats, piston guides, silding rails, ring seals, bearing discs, bearingsInformation Provided by Ensinger, Inc.
Physical Properties Metric English Comments
Density 1.88 g/cc

@Temperature 23.0 °C
0.0679 lb/in³

@Temperature 73.4 °F
DIN 53 479
Filler Content 20 %
20 %
PI
Water Absorption 0.70 %

@Temperature 23.0 °C,
Time 86400 sec
0.70 %

@Temperature 73.4 °F,
Time 24.0 hour
EN ISO 62
Mechanical Properties Metric English Comments
Hardness, Shore D 65

@Temperature 23.0 °C
65

@Temperature 73.4 °F
DIN 53 505
Tensile Strength, Yield 15.0 MPa

@Temperature 23.0 °C
2180 psi

@Temperature 73.4 °F
EN ISO 527
Elongation at Break 200 %

@Temperature 23.0 °C
200 %

@Temperature 73.4 °F
EN ISO 527
Thermal Properties Metric English Comments
CTE, linear 144 µm/m-°C

@Temperature 50.0 - 200 °C
80.0 µin/in-°F

@Temperature 122 - 392 °F
DIN 53 752
Specific Heat Capacity 1.00 J/g-°C
0.239 BTU/lb-°F
Thermal Conductivity 0.250 W/m-K

@Temperature 40.0 °C
1.74 BTU-in/hr-ft²-°F

@Temperature 104 °F
ISO 8302
Glass Transition Temp, Tg -20.0 °C
-4.00 °F
DMTA
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+18 ohm-cm

@Temperature 23.0 °C
1.00e+18 ohm-cm

@Temperature 73.4 °F
IEC 60093
Dielectric Constant 2.3

@Frequency 10000 Hz,
Temperature 23.0 °C
2.3

@Frequency 10000 Hz,
Temperature 73.4 °F
IEC 60250
Descriptive Properties Value Comments
Color Ochre Brown
DIN-Abbreviation TF PI
Copyright © lookpolymers.com All Rights Reserved