Material Notes:
HYDEL® PC-P ESD polycarbonate is a static dissipative thermoplastic product containing carbon powder. This material has good stiffness, excellent dimensional ability, and low outgassing properties.Information Provided by Ensinger Industries, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.34 g/cc
1.34 g/cc
ASTM D792
Water Absorption 0.10 %

@Temperature 22.8 °C,
Time 86400 sec
0.10 %

@Temperature 73.0 °F,
Time 24.0 hour
ASTM D570
Mechanical Properties Metric English Comments
Tensile Strength, Yield 65.5 MPa
9500 psi
ASTM D638
Elongation at Break 5.0 %
5.0 %
ASTM D638
Tensile Modulus 2.07 GPa
300 ksi
ASTM D638
Flexural Strength 107 MPa
15500 psi
ASTM D790
Flexural Modulus 2.34 GPa
340 ksi
ASTM D790
Izod Impact, Notched 0.801 J/cm
1.50 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 132 °C
270 °F
continuous
Deflection Temperature at 1.8 MPa (264 psi) 132 °C
270 °F
ASTM D648
Flammability, UL94 V-2
V-2
Electrical Properties Metric English Comments
Surface Resistivity per Square 1.00e+7 - 1.00e+12 ohm
1.00e+7 - 1.00e+12 ohm
ASTM D257
Descriptive Properties Value Comments
Base Material Polycarbonate