Ensinger ENSITEP® PET Polyethylene Terephthalate - Extruded Products  (discontinued **)

Category Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET)
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ensinger ENSITEP® PET Polyethylene Terephthalate - Extruded Products  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
ENSITEP is an unreinforced, semi-crystalline thermoplastic polyester derived from polyethylene terephthalate. Its excellent wear resistance, low coefficient of friction, high flexural modulus, and superior dimensional stability make it a versatile material for designing mechanical and electro-mechanical parts. Because ENSITEP has no centerline porosity, the possibility of fluid absorption and leakage is virtually eliminated. Uses: ENSITEP's superior wear resistance and lack of centerline porosity give it an advantage over other materials for applications involving solvents, chemicals, and food products. ENSITEP is also used in water purification systems, printing equipment, textile components, food-handling equipment, and valves.Information supplied by Ensinger, Inc.Ensitep grades have been replaced by Tecapet
Physical Properties Metric English Comments
Density 1.38 g/cc
0.0499 lb/in³
ASTM D792
Water Absorption 0.10 %
0.10 %
at 24 hours; ASTM D570
Water Absorption at Saturation 0.50 %
0.50 %
ASTM D570
Mechanical Properties Metric English Comments
Hardness, Rockwell R 114
114
ASTM D785
Tensile Strength, Yield 79.3 MPa
11500 psi
ASTM D638
Elongation at Break 15 %
15 %
ASTM D638
Tensile Modulus 2.76 GPa
400 ksi
ASTM D638
Flexural Strength 109 MPa
15800 psi
ASTM D790
Flexural Modulus 2.83 GPa
411 ksi
ASTM D790
Compressive Strength 35.9 MPa
5200 psi
ASTM D695
Izod Impact, Notched 0.320 J/cm
0.600 ft-lb/in
ASTM D256
Coefficient of Friction, Dynamic 0.25
0.25
40 psi, 50 fpm; ASTM D3702
Coefficient of Friction, Static 0.19
0.19
ASTM D3702
K (wear) Factor 423 x 10-8 mm³/N-M
210 x 10-10 in³-min/ft-lb-hr
40 psi, 50 fpm; ASTM D3702
Thermal Properties Metric English Comments
CTE, linear 70.2 µm/m-°C

@Temperature 20.0 °C
39.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Specific Heat Capacity 1.17 J/g-°C
0.280 BTU/lb-°F
Thermal Conductivity 0.290 W/m-K
2.01 BTU-in/hr-ft²-°F
Melting Point 254 °C
490 °F
ASTM D2133
Maximum Service Temperature, Air 110 °C
230 °F
Long Term; ASTM UL746B
160 °C
320 °F
Intermittent
Deflection Temperature at 0.46 MPa (66 psi) 116 °C
240 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 79.4 °C
175 °F
ASTM D648
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
ASTM D257
Dielectric Constant 3.4

@Frequency 60 Hz
3.4

@Frequency 60 Hz
50% RH; ASTM D150
3.7

@Frequency 60 Hz
3.7

@Frequency 60 Hz
ASTM D150
Dielectric Strength 15.7 kV/mm
400 kV/in
ASTM D149
Dissipation Factor 0.0020

@Frequency 60 Hz
0.0020

@Frequency 60 Hz
ASTM D150