Ensinger DELRIN® 507 Black Acetal Homopolymer (POM)

Category Polymer , Thermoplastic , Acetal (POM) , Acetal Homopolymer, Unreinforced
Manufacturer Ensinger
Trade Name Delrin®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ensinger DELRIN® 507 Black Acetal Homopolymer (POM).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Delrin® 507 is a general purpose homopolymer acetal containing a UV stabilizer ideally suited for outdoor applications or those in which there is an otherwise abundant source of UV light.General higher surface hardnessEasily machinableDesigned for outdoor applicationsDelrin 507 Black is typically used for outdoor applications in such industries as electronics, communications, transportation, construction and marine.Information provided by Ensinger
Physical Properties Metric English Comments
Specific Gravity 1.40 g/cc
1.40 g/cc
ASTM D792
Water Absorption 0.20 %

@Time 86400 sec
0.20 %

@Time 24.0 hour
ASTM D570
Mechanical Properties Metric English Comments
Hardness, Rockwell M 91
91
ASTM D785
Hardness, Rockwell R 120
120
ASTM D785
Tensile Strength, Yield 70.60 MPa
10240 psi
ASTM D638
Elongation at Break 10 %
10 %
ASTM D638
Tensile Modulus 2.52 GPa
366 ksi
ASTM D638
Flexural Strength 134 MPa
19400 psi
ASTM D790
Flexural Modulus 3.32 GPa
482 ksi
ASTM D790
Izod Impact, Notched 0.683 J/cm
1.28 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 175 °C
347 °F
ASTM D3418
Maximum Service Temperature, Air 93.3 °C
200 °F
long term; ASTM D648
Deflection Temperature at 0.46 MPa (66 psi) 169 °C
336 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 114 °C
237 °F
ASTM D648
Users viewing this material also viewed the following: