Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Engineered Plastics EP Alloy 510B PC/ABS Alloy

Category Polymer , Thermoplastic , ABS Polymer , Polycarbonate/ABS Alloy, Unreinforced , Polycarbonate (PC)
Manufacturer Engineered Plastics Corporation
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Engineered Plastics EP Alloy 510B PC/ABS Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Gray. Stiff tough and excellent color stability. Used in housings for computers, printers, copiers and for auto parts such as air ducts and instrument panels. GMP # 002; Ford # WSS585. Property values below represent typical values; black, gray, ext/inj grades and FR/non FR grades are available and can be tailored to meet specific requirements. Information provided by Engineered Plastics Corporation.
Physical Properties Metric English Comments
Density 1.16 g/cc
0.0419 lb/in³
ASTM D792
Melt Flow 5.5 g/10 min
5.5 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 56.0 MPa
8120 psi
ASTM D638
Elongation at Break 125 %
125 %
ASTM D638
Flexural Modulus 2.31 GPa
335 ksi
ASTM D790
Izod Impact, Notched 5.90 J/cm
11.1 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 110 °C
230 °F
Annealed; ASTM Data
113 °C
235 °F
Unannealed; ASTM Data
Vicat Softening Point 113 °C
235 °F
ASTM D1525
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in