Elisto THERMOSTAR® MD 80 Pattern material

Category Other Engineering Material
Manufacturer Elisto
Trade Name THERMOSTAR®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Elisto THERMOSTAR® MD 80 Pattern material.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Block materialInformation provided by elisto
Physical Properties Metric English Comments
Specific Gravity 0.800 g/cc
0.800 g/cc
Water Absorption 0.20 %
0.20 %
Mechanical Properties Metric English Comments
Flexural Strength 27.0 MPa

@Temperature 23.0 °C
3920 psi

@Temperature 73.4 °F
Flexural Modulus 2.20 GPa
319 ksi
Compressive Strength 30.0 MPa

@Temperature 23.0 °C
4350 psi

@Temperature 73.4 °F
Descriptive Properties Value Comments
Application Temperature (°C) 230