Eliokem Chemigum® P83 Nitrile Elastomer

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Eliokem
Trade Name Chemigum®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Eliokem Chemigum® P83 Nitrile Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Balanced modifier of plasticized PVC for improved properties and melt processing in the Eliokem product line. 33% bound ACN. Crosslinked polymer structure. PVC partitioning agent.Can be used in PVC blends.Used in automotive (interior moldings, decorative profiles/spoilers, oil and gas resistant parts), glazing gaskets, roofing membranes, flooring, footwear, cable jacketing, hoses and tubing, appliance gaskets/profiles, and synthetic leather.Information provided by Eliokem.
Physical Properties Metric English Comments
Density 1.00 g/cc
0.0361 lb/in³
Particle Size 600 µm
600 µm
Median
Mooney Viscosity 57

@Temperature 100 °C
57

@Temperature 212 °F
ML 1+4