Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Elastomer Engineering Elastamide 100 Elastomer Modified RIM Nylon 6

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Impact Grade
Manufacturer Elastomer Engineering
Trade Name Elastamide
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Elastomer Engineering Elastamide 100 Elastomer Modified RIM Nylon 6.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
30% crystallinity. Information supplied by Elastomer Engineering.
Physical Properties Metric English Comments
Water Absorption 3.1 %
3.1 %
24 hrs; DIN 53714
Mechanical Properties Metric English Comments
Hardness, Shore D 74
74
Tensile Strength, Ultimate 49.0 MPa
7110 psi
ASTM D638
Elongation at Break 250 %
250 %
ASTM D638
Tensile Modulus 1.20 GPa
174 ksi
ASTM D638
Flexural Modulus 1.17 GPa
170 ksi
ASTM D790
Izod Impact, Notched 3.52 J/cm
6.59 ft-lb/in
Method B; Ductile Failure
0.430 J/cm

@Temperature -40.0 °C
0.806 ft-lb/in

@Temperature -40.0 °F
Method B; Brittle Failure
Charpy Impact, Notched 1.20 J/cm²
5.71 ft-lb/in²
Brittle Failure; ASTM D256B
0.310 J/cm²

@Temperature -40.0 °C
1.48 ft-lb/in²

@Temperature -40.0 °F
Method B; Brittle Failure
Taber Abrasion, mg/1000 Cycles 10
10
Electrical Properties Metric English Comments
Dielectric Constant 4.1

@Frequency 100000 Hz
4.1

@Frequency 100000 Hz
7.9

@Frequency 1000 Hz
7.9

@Frequency 1000 Hz
15.3

@Frequency 50 Hz
15.3

@Frequency 50 Hz
Dielectric Strength 13.0 kV/mm
330 kV/in
Dissipation Factor 0.10

@Frequency 100000 Hz
0.10

@Frequency 100000 Hz
ASTM D150
0.30

@Frequency 1000 Hz
0.30

@Frequency 1000 Hz
ASTM D150
Comparative Tracking Index 400 V
400 V
ASTM D257
Copyright © lookpolymers.com All Rights Reserved