Elastomer Engineering E60D Polyurethane

Category Polymer , Thermoplastic , Polyester, TP , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Polyester Grade
Manufacturer Elastomer Engineering
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Elastomer Engineering E60D Polyurethane.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A polyester-based urethane with particularly high load-bearing characteristics. Information provided by Elastomer Engineering Inc (EEI)
Mechanical Properties Metric English Comments
Hardness, Shore D 61
61
Tensile Strength, Ultimate 51.0 MPa
7400 psi
Elongation at Break 415 %
415 %
100% Modulus 0.0200 GPa
2.90 ksi
300% Modulus 0.0303 GPa
4.40 ksi
Rebound 33 %
33 %
Bayshore
Tear Strength 78.9 kN/m
450 pli
Split
126 kN/m
720 pli
Die C
Compression Set 34 %
34 %
Method B