Elastomer Engineering E57L Polyurethane

Category Polymer , Thermoplastic , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Polyether Grade
Manufacturer Elastomer Engineering
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Elastomer Engineering E57L Polyurethane.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
An extremely hard, rigid polyether based elastomer. This material fills the gap between rigid plastic and flexible rubber-like materials. Its unique properties of self-lubrication and shock-resistance make it a natural for bushings, bearings, and machined parts. Information provided by Elastomer Engineering Inc (EEI)
Mechanical Properties Metric English Comments
Hardness, Shore D 75 - 78
75 - 78
Tensile Strength, Ultimate 68.9 MPa
10000 psi
Elongation at Break 210 %
210 %
Rebound 45 %
45 %
Bayshore
Compression Set 1.0 %
1.0 %
Method A