Eifeler Coatings Technology VARIANTA® TiAlN PVD Coating

Category Ceramic , Nitride , Other Engineering Material , Ceramic/Metallic Coating
Manufacturer Eifeler Coatings Technology
Trade Name VARIANTA®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Eifeler Coatings Technology VARIANTA® TiAlN PVD Coating.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Key Characteristics: high hardness, very good oxidation resistancePrimary Applications: coating for a wide range of carbide, cermet and high speed steel tools; machining of cast iron and nickel based high temperature alloys; high speed operations, semi-dry or dry machining, orthopedic instrumentationInformation provided by Eifeler Coatings Technology
Physical Properties Metric English Comments
Thickness 2.00 - 4.00 microns
0.0787 - 0.157 mil
Mechanical Properties Metric English Comments
Vickers Microhardness 3000 - 4000
3000 - 4000
Coefficient of Friction 0.70
0.70
dry, steel
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 800 °C
1470 °F
Descriptive Properties Value Comments
Color anthracite