Material Notes:
Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applications.High Specific GravityTungsten Powder Filled SEBS Base ResinVery FlexibleInformation provided by Technical Polymers
Physical Properties Metric English Comments
Specific Gravity 11.0 g/cc
11.0 g/cc
ASTM D792
Linear Mold Shrinkage 0.0030 - 0.0050 cm/cm
0.0030 - 0.0050 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Shore D 23
23
ASTM D2240
Tensile Strength, Ultimate 1.35 MPa
196 psi
ASTM D638
Elongation at Break 177 %
177 %
ASTM D638
Flexural Strength 2.66 MPa
386 psi
ASTM D790
Flexural Modulus 0.0917 GPa
13.3 ksi
ASTM D790
Izod Impact, Notched 1.07 J/cm
2.00 ft-lb/in
ASTM D256
Processing Properties Metric English Comments
Melt Temperature 149 - 204 °C
300 - 400 °F
Mold Temperature 21.1 - 37.8 °C
70.0 - 100 °F