Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Eastman Ecdel PCCE 9965 Copolyester Ether Elastomer

Category Polymer , Thermoplastic , Polyester, TP
Manufacturer Eastman Chemical
Trade Name Ecdel
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Eastman Ecdel PCCE 9965 Copolyester Ether Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
ISO data as provided by the manufacturer, Eastman Chemical
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Yield 12.0 MPa
1740 psi
50 mm/min
Elongation at Break >= 50 %
>= 50 %
Elongation at Yield 29 %
29 %
Tensile Modulus 0.156 GPa
22.6 ksi
1mm/min
Charpy Impact Unnotched NB
NB
NB

@Temperature -30.0 °C
NB

@Temperature -22.0 °F
Charpy Impact, Notched NB
NB
1.10 J/cm²

@Temperature -30.0 °C
5.24 ft-lb/in²

@Temperature -22.0 °F
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 148 µm/m-°C

@Temperature 20.0 °C
82.2 µin/in-°F

@Temperature 68.0 °F
CTE, linear, Transverse to Flow 139 µm/m-°C

@Temperature 20.0 °C
77.2 µin/in-°F

@Temperature 68.0 °F
Melting Point 208 °C
406 °F
Deflection Temperature at 0.46 MPa (66 psi) 57.0 °C
135 °F
Deflection Temperature at 1.8 MPa (264 psi) 46.0 °C
115 °F
Vicat Softening Point 56.0 °C
133 °F
Glass Transition Temp, Tg -3.00 °C
26.6 °F
Processing Properties Metric English Comments
Melt Temperature 225 - 260 °C
437 - 500 °F
Users viewing this material also viewed the following: