Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Eastman Eastar GN125 Copolyester, Natural  (discontinued **)

Category Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET) , Polyethylene Terephthalate (PET), Unreinforced
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Eastman Eastar GN125 Copolyester, Natural  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Eastar Copolyester GN125 is a glycol modified polyethylene terephthalate (PET) that contains an ultraviolet light inhibitor. This product is recommended for indoor applications requiring enhanced color stability. Eastar copolyester GN125 will not crystallize and as a result, offers a wider processing latitude than conventional crystallizable polyesters. This product offers an excellent combination of clarity, toughness, and melt strength that makes if useful for a variety of processing techniques and end-use applications.Applications/UsesCosmetics/personal care packagingWriting InstrumentsPoint of purchase displaysToys/Sporting goodsLighting
Physical Properties Metric English Comments
Specific Gravity 1.30 g/cc
1.30 g/cc
ASTM D792
Water Absorption 0.13 %
0.13 %
24h Immersion; ASTM D570
Linear Mold Shrinkage 0.0020 - 0.0050 cm/cm

@Thickness 3.20 mm
0.0020 - 0.0050 in/in

@Thickness 0.126 in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 106
106
ASTM D785
Tensile Strength at Break 27.0 MPa
3920 psi
ISO 527
30.0 MPa
4350 psi
ASTM D638
Tensile Strength, Yield 49.0 MPa
7110 psi
ASTM D638
49.0 MPa
7110 psi
ISO 527
Elongation at Break 110 %
110 %
ISO 527
150 %
150 %
ASTM D638
Elongation at Yield 4.0 %
4.0 %
ISO 527
4.3 %
4.3 %
ASTM D638
Tensile Modulus 2.01 GPa
292 ksi
ASTM D638
2.02 GPa
293 ksi
ISO 527
Flexural Strength 69.0 MPa
10000 psi
ISO 178
71.0 MPa
10300 psi
ASTM D790
Flexural Modulus 2.10 GPa
305 ksi
ISO 178
2.20 GPa
319 ksi
ASTM D790
Izod Impact, Notched 0.270 J/cm

@Temperature -40.0 °C
0.506 ft-lb/in

@Temperature -40.0 °F
ASTM D256
0.980 J/cm

@Temperature 23.0 °C
1.84 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Izod Impact, Unnotched NB
NB
ASTM D4812
NB

@Temperature -40.0 °C
NB

@Temperature -40.0 °F
ASTM D4812
Izod Impact, Notched (ISO) 3.90 kJ/m²

@Temperature -40.0 °C
1.86 ft-lb/in²

@Temperature -40.0 °F
ISO 180
8.10 kJ/m²

@Temperature 23.0 °C
3.85 ft-lb/in²

@Temperature 73.4 °F
ISO 180
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 69.0 °C
156 °F
ISO 75
69.0 °C
156 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °C
140 °F
ASTM D648
62.0 °C
144 °F
ISO 75
Optical Properties Metric English Comments
Haze 0.30 %
0.30 %
ASTM D1003
Transmission, Visible 91 %
91 %
Total Transmittance; ASTM D1003
Processing Properties Metric English Comments
Melt Temperature 249 - 271 °C
480 - 520 °F
Mold Temperature 16.0 - 38.0 °C
60.8 - 100 °F
Drying Temperature 71.0 °C
160 °F
Dry Time 4 - 6 hour
4 - 6 hour