Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Eastman Eastar Copolyester K3000 PETG Copolyester  (discontinued **)

Category Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET) , PETG Copolyester
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Eastman Eastar Copolyester K3000 PETG Copolyester  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
EASTAR K3000 Copolyester is a cost effective, high-performance, water-clear material that provides the necessary performance for the appliance standards. Other desirable characteristics are good chemical resistance, stiffness, and low shrinkage. In addition, it is "molder friendly" and colors and tints easily.Applications: Refrigerator interior partsTechnical Data Sheet Comments: Properties reported here are typical of average lots. Eastman makes no representation that the material in any particular shipment will conform to the values giveInformation provided by Eastman Chemical.
Physical Properties Metric English Comments
Density 1.31 g/cc
0.0473 lb/in³
ASTM D792
Linear Mold Shrinkage, Flow 0.0050 cm/cm

@Thickness 3.20 mm
0.0050 in/in

@Thickness 0.126 in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 105
105
ASTM D785
Tensile Strength, Ultimate 26.0 MPa
3770 psi
ASTM D638
26.0 MPa
3770 psi
ISO 527
Tensile Strength, Yield 53.0 MPa
7690 psi
ASTM D638
54.0 MPa
7830 psi
ISO 527
Elongation at Break 61 %
61 %
ISO 527
Elongation at Yield 4.0 %
4.0 %
ISO 527
Tensile Modulus 2.02 GPa
293 ksi
ISO 527
Flexural Yield Strength 74.0 MPa
10700 psi
ISO 178
77.0 MPa
11200 psi
ASTM D790
Flexural Modulus 2.34 GPa
339 ksi
ISO 178
Izod Impact, Notched 0.590 J/cm
1.11 ft-lb/in
ASTM D256
0.290 J/cm

@Temperature -40.0 °C
0.543 ft-lb/in

@Temperature -40.0 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 68.0 °C
154 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 61.0 °C
142 °F
ASTM D648
Optical Properties Metric English Comments
Haze 0.50 %
0.50 %
ASTM D1003
Transmission, Visible 89 %
89 %
Regular transmittance per ASTM D 1003
91 %
91 %
Total Transmittance; ASTM D 1003
Processing Properties Metric English Comments
Melt Temperature 282 °C
540 °F
Mold Temperature 27.0 °C
80.6 °F
Drying Temperature 102 °C
216 °F
Dry Time 4 hour
4 hour